Petter Stahre
New member
I just recieved two boxes (my first) of the Innova F-type Gloss paper.
When I opened one box and inspected the paper it looked as if the first 5-6 papers had scruff marks on them. I then noticed the idiotic plastic packaging. It seals itself with three hard plastic edges just at the middle of the sheets (not at the sides) - exactly the same place as the scruff marks. This means that when the paper is shipped, or the boxes are stacked, the plastic details will scratch the sheets. And it's the coated printing side that is damaged.
The other box had the same problem, as expected. What where they thinking at Innova?
But the real problem (aside of wasting 5-6 sheets out of 25 per box!) is that when I look at the coating of the unscruffed papers I find it to be quite uneven (varying from a little to quite much). Compared to the coating of both the Crane Museo SilverRag and Hahnemuhle FineArt Pearl, which I also have, Innova seems to have quality issues with their production.
Or is it just my batch? Have others remarked on this - uneven coating?
Cheers,
Petter
When I opened one box and inspected the paper it looked as if the first 5-6 papers had scruff marks on them. I then noticed the idiotic plastic packaging. It seals itself with three hard plastic edges just at the middle of the sheets (not at the sides) - exactly the same place as the scruff marks. This means that when the paper is shipped, or the boxes are stacked, the plastic details will scratch the sheets. And it's the coated printing side that is damaged.
The other box had the same problem, as expected. What where they thinking at Innova?
But the real problem (aside of wasting 5-6 sheets out of 25 per box!) is that when I look at the coating of the unscruffed papers I find it to be quite uneven (varying from a little to quite much). Compared to the coating of both the Crane Museo SilverRag and Hahnemuhle FineArt Pearl, which I also have, Innova seems to have quality issues with their production.
Or is it just my batch? Have others remarked on this - uneven coating?
Cheers,
Petter